Availability: | |
---|---|
NKS-10kVRSG- NKS-20kVRSG- NKS-35kVRSG-
NKS POWER
Medium Voltage Heat Shrink Tubing product introduction:
Heat shrinkable busbar bushings are used for insulation protection of busbar copper bars in up to 42kV substation distribution cabinets and other places. It has good anti-fouling, flame retardant, corrosion resistance and insulation properties, providing a strong guarantee for the safe operation of the power system.
Working temperature -55℃~125℃; shrinkage temperature 85~100℃, complete shrinkage temperature 130℃.
Medium Voltage heat shrink tubing product features:
High mechanical strength, suitable for a variety of power cables
Strong UV resistance and strong weather resistance
Has excellent insulation properties, corona resistance and tracking resistance
Simple design and reasonable structure
Electrical performance parameters of Medium Voltage heat shrink tubing:
Test Items | Test Methods | Test Requirements |
Tensile Strength | ASTM D638 | ≥10Mpa |
Ultimate elongation | ASTM D638 | ≥300% |
Tensile Strength after Aging | ASTM D638 | ≥8Mpa |
Ultimate elongation after aging | ASTM D638 | ≥250% |
Longitudinal shrinkage | ASTM D2671 | ±5% |
Dielectric constant | ASTM D2671 | ≥18Ω.cm |
voltage breakdown strength | ASTM D149 | ≥25kv/mm |
Volume resistivity | ASTM D257 | >1014Ω.cm |
density | ASTM D792 | 1.22g/cm² |
Flame retardancy | UL 224 | VW-1 |
complete shrinkage temperature | ASTM D792 | 130±5℃ |
Selection table for Medium Voltage heat shrink tubing:
Medium Voltage Heat Shrink Tubing product introduction:
Heat shrinkable busbar bushings are used for insulation protection of busbar copper bars in up to 42kV substation distribution cabinets and other places. It has good anti-fouling, flame retardant, corrosion resistance and insulation properties, providing a strong guarantee for the safe operation of the power system.
Working temperature -55℃~125℃; shrinkage temperature 85~100℃, complete shrinkage temperature 130℃.
Medium Voltage heat shrink tubing product features:
High mechanical strength, suitable for a variety of power cables
Strong UV resistance and strong weather resistance
Has excellent insulation properties, corona resistance and tracking resistance
Simple design and reasonable structure
Electrical performance parameters of Medium Voltage heat shrink tubing:
Test Items | Test Methods | Test Requirements |
Tensile Strength | ASTM D638 | ≥10Mpa |
Ultimate elongation | ASTM D638 | ≥300% |
Tensile Strength after Aging | ASTM D638 | ≥8Mpa |
Ultimate elongation after aging | ASTM D638 | ≥250% |
Longitudinal shrinkage | ASTM D2671 | ±5% |
Dielectric constant | ASTM D2671 | ≥18Ω.cm |
voltage breakdown strength | ASTM D149 | ≥25kv/mm |
Volume resistivity | ASTM D257 | >1014Ω.cm |
density | ASTM D792 | 1.22g/cm² |
Flame retardancy | UL 224 | VW-1 |
complete shrinkage temperature | ASTM D792 | 130±5℃ |
Selection table for Medium Voltage heat shrink tubing: